Udimet 720 Superalloy Powder
Udimet 720 is a precipitation hardened nickel based superalloy known as its excellent high temperature strength, creep resistance, and oxidation resistance.
Udimet 720 can get the density up to 8.08g/cm3, melting point of 1371℃ and thermal expansion coefficient 12.24um/m℃ at 93℃. It can be used in aerospace turbine, hotsection
components.
Fast Delivery
High sphericity
High Quality
Small MOQ
Share This Product
Product Description
Udimet 720 Superalloy Powder
Udimet 720 is a precipitation hardened nickel based superalloy known as its excellent high temperature strength, creep resistance, and oxidation resistance.
Udimet 720 can get the density up to 8.08g/cm3, melting point of 1371℃ and thermal expansion coefficient 12.24um/m℃ at 93℃. It can be used in aerospace turbine, hotsection
components.
AF-9628 is a steel alloy developed by AFRL’s Dr. Rachel Abrahams that offers high strength and toughness. AF9628 is low alloy martensitic steel with the strength greater than 1.5 GPa due to the formation of ε-carbide phase and excellent toughness at -40°F.
Chemical Composition

Morphology

Powder Property (PSD 0-25um):

We also can provide customized different particle size distribution. Please contact us.
Package:

PREP System
AM Powder
Sent Inquiry
Any questions? Send us message now! We’ll serve your request with a whole team after receiving your message.
Related products
-

Al 7075 powder
Al 7075 powder is a high-strength aluminum alloy composed primarily…
-

Ti22Al25Nb Powder
Ti22Al25Nb powder is an innovative alloy powder composed of titanium…
-

TC11 Powder : A Comprehensive Guide
TC11 powder, also known as Titanium Carbide 11, is a…
-

Best Hastelloy X Powder丨High temperature alloy Powder for 3D Printing
Hastelloy X Powder holds a special place. It’s a nickel-based…
Applications
How we play a role in the industry
HIP Technology
Hot Isostatic Pressing (HIP) technology works by placing the product in a closed container, filling it with inert gas and sintering or densifying the product at a very high temperature (usually close to the forging temperature of the material) and at a very high pressure (usually 100 – 140 MPa). This allows the product to be sintered or densified.
MIM Technology
MIM products can be complex in shape, precise in size, high in strength and produced automatically in large quantities, and can significantly reduce the complexity and cost of traditional metalworking
SLM Technology
SLM, also known as Selective Laser Melting, is similar in principle to SLS in that a laser is used to melt and solidify metal powder in a specified area, which is then moulded in a layer-by-layer stack.
EBM Technology
Electron beam melting refers to a vacuum melting method in which the kinetic energy of a high speed electron beam stream is converted to heat as a heat source for melting metals under high vacuum. The abbreviation is EBM.
POPULAR SERVICE
Our Professional Services
For Additive Manufacturing
Various Products
Here we provide more than 40 grades of high-quality powders.
3D Printing
SEBM&PREP technology and equipment.
Customization
Accept OEM/ODM
No Risk
Perfect supply chain layout
High Quality
Top sales and quality
Fair Prices
High quality products at reasonable prices
Send Inquiry
Thank you for your interest in our products. If you have any enquiry about quotation or cooperation, please feel free to leave us message by using the following enquiry form. Our sales representative will contact you within 24 hours.